still not hot enough

So the redo up to 1275 was very nice for the turquoise mask... the big chunks are nicely welded together but are still chunky. However, the tack fusing on the system 96 masks still looks, well, tacky. So those ones are currently cooking again. This time up to 1305. And a slower ramp from 1000 to 1305 because I am foolishly also cooking two clay molds.

we shall see what happens tomorrow a.m.